MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Synfoam® LG-10 Syntactic Foam
Categories: Polymer; Thermoset

Material Notes: Castable. SynFoam LG is a unique, expandable, closed cell syntactic foam that provides very low density and moderate strength. SynFoam LG is an ideal replacement for polyurethane foams where higher modulus is needed to support lightweight structures. It is suitable for numerous marine and aerospace applications or where machining of parts is either impractical or too expensive. SynFoam LG is available as 1, 2, and 5 gallon kits. Each kit contains an A and B side that must be mixed together prior to casting. Cure is achieved within 24 hours and full properties will be realized after 7 days at room temperature. Densities can be customized to the user's specifications. Interlayer adhesion allowing large structures to be made with multiple pours.

Information provided by Synfoam®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.128 - 0.192 g/cc0.00463 - 0.00694 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 2.07 MPa300 psi
Compressive Modulus 0.0414 GPa6.00 ksi
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 95.0 °C203 °F
 
Descriptive Properties
Depth Rating (m)150

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Norplex-Micarta ES1 Melamine Paper Laminate Sheet, NEMA ES-1

PSYNF037 / 192912

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.