MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Michelman® Michem® Flex P1801 Water based primer  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Water based primer for liquids and extrusion coated resins.

Usage: Michem®Flex P1801 is a primer for film and paper substrates to promote adhesion to extrusion coated resins resulting in excellent bond strength. Suitable for bioplastic substrates and extrudates, as well as resins extruded at low temperatures. This product has been formulated with non-petroleum based content.

Application Data: Michem®Flex P1801 may be applied via flexo, gravure or smooth roll coater. Corona or flame treat substrates prior to priming and dry thoroughly with hot, circulating air. This product is best for in-line processes, as it may block in rewound rolls. Recommended application weight for film substrates is between 0.1 - 1.0 dry g/m2.

When manufactured in the USA Product meets food contact regulations for:
Europe: Euro. Res. AP(2004)1 (Restricted) and Commission Regulation (EU) n° 10/2011(Restricted)

Food Contact Information when manufactured in the USA:
FDA:
175.105: Components of adhesives. (Restricted).
175.300: Resinous and polymeric components of coatings(Restricted)
175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods. (Restricted)

When manufactured in Belgium product meets food contact regulations for:
Europe: Euro. Res. AP(2004)1 (Restricted) and Commission Regulation (EU) n° 10/2011(Restricted)
Germany: BfR Recommendation XIV (Restricted)and BfR Recommendation XXXVI (Restricted)

Food Contact Information when manufactured in Belgium:
FDA:
175.105: Components of adhesives. (Restricted).
175.300: Resinous and polymeric components of coatings(Restricted)
175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted)
176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods. (Restricted)

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 - 1.02 g/cc
Volatiles 74 - 76 %
pH 8.0 - 10
Brookfield Viscosity <= 500 cPSpindle # 3, rpm 60
 
Descriptive Properties
AppearanceThin, translucent, amber colored liquid

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WMICHEL119 / 135036

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.