MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChevronTexaco Capella® WF 100
Categories: Fluid; Lubricant

Material Notes: Texaco Capella WF oils delivers value through:
  • Wax-free — Suitable for ultra-low temperature service.
  • Water-free — Low moisture content prevents icing in refrigeration expansion valves and helps prevent system corrosion.
  • Low carbon residue — Reduces the tendency to form carbon deposits on the hot spots of the compressor unit.
  • Excellent compatibility in both Freon®1 and ammonia systems — Suitable for use in many types of refrigeration systems. Meets all Carrier and Elsey tests for stability and refrigerant compatibility.
  • Premium quality — Virtually eliminates lubricant caused equipment failures.
  • Thermal stability — For long service life.

Texaco Capella WF oils provide maximum wear protection to any refrigeration compressor or system in which they are used.

Texaco Capella WF oils are manufactured using specially refined naphthenic mineral oils. Carefully selected base stocks assure the low pour points necessary for refrigeration compressor lubricants.

They are highly refined and specially treated to resist the sludging action of refrigerants in the presence of high temperature and metal catalysts.

Texaco Capella WF oils are suitable for use in any refrigeration system. They are particularly suitable for modern, compact, high pressure refrigeration systems using Freon. Since they are wax-free, they are suitable for use in very cold ambient temperatures as a bearing lubricant or for hand oiling.

Texaco Capella WF oils are unsuitable for refrigerant systems using HFC refrigerants, such as R-134a.

The viscosity grade for the application should be based on the equipment manufacturers recommendation.

Texaco Capella WF oils satisfy the requirements of hermetically sealed air conditioning compressors or the many types of smaller units.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 220768; MSDS Number: 8824

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 23.1 °23.1 °
Viscosity Measurement 3535Viscosity Index
Saybolt Viscosity at 100°F 526 SUS526 SUS
Saybolt Viscosity at 210°F 56 SUS56 SUS
Kinematic Viscosity at 40°C (104°F) 99 cSt99 cSt
Kinematic Viscosity at 100°C (212°F) 8.7 cSt8.7 cSt
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 30.0 kV/mm
@Thickness 1.00 mm
>= 762 kV/in
@Thickness 0.0394 in
 
Thermal PropertiesMetricEnglishComments
Pour Point -29.0 °C-20.2 °F
Flash Point 213 °C415 °F
 
Descriptive Properties
Sealed Tube Stability %1.3R-22, 14 days

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WTEXA038 / 76917

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.