MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® 510 Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: Weatherable and decorative sheet

KYDEX® 510 is a weatherable sheet with superior performance for thermoforming and a decorative sheet for lamination.

KYDEX® 510 is available in many distinctive colors and textures. An acrylic cap protects the surface, providing excellent weatherability for outdoor use. This product is now available with decorative film (black/white granite). While excellent in thermoforming, KYDEX® 510 is also being used as damage resistant surface material.

Suggested Applications:

  • Kiosk Housings
  • Equipment Housings
  • Medical Products
  • Miscellaneous Applications

Features:

  • Offers same properties of KYDEX® sheet, but in a weatherable formula
  • Highly impact resistant as measured by the Notched Izod Impact Resistance test
  • Fire retardant (self-extinguishing) with UL Std 94 V-0 and 5V ratings
  • Low moisture absorption, resistance to chipping and cracking, great fabrication and machining properties and flexibility and flexibility
  • Excellent forming properties, uniform wall thickness and crisp detail
  • Can be drilled, punched and cut using standard woodworking or metal working tools
  • Exhibits a Dielectric Constant of 2.76 @ 100 Hz, 2.53 @ 800 MHz and 2.51 @ 1.9 GHz

Values based upon 3.18 mm (0.125 in) sheet unless otherwise specified.

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 94ASTM D785
Tensile Strength 42.0 MPaASTM D638
Modulus of Elasticity 2.48 GPaASTM D790
Flexural Strength 66.0 MPaASTM D790
Izod Impact, Notched 801 J/m
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 38.3 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 168 °FAnnealed; ASTM D648
Flammability, UL94 V-0UL Component Recognition
 5VB
@Thickness >=0.991 mm
Underwriters Laboratories., Inc®; Component Recognition; UL Standard 94
 
Processing PropertiesOriginal ValueComments
Processing Temperature 325 - 390 °FForming Temperature
 
Descriptive Properties
FlammabilityClass 1 (1 mm)BS 476 Part 7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® T Thermoplastic
SEKISUI SPI KYDEX® 110 Polymer Alloy Sheet
SEKISUI SPI KYDEX® 100 Polymer Alloy Sheet
SEKISUI SPI KYDEX® 410 ABS/PVC
SEKISUI SPI KYDEX® 430 ABS/PVC

PSEKIS034 / 185859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.