Temper: As Sand Cast Casting Characteristics: High –Drossing; Medium – Casting Yield, Shrinkage in Solidification; Low – Effect of Section Size, Fluidity, Gassing Fabrication Properties: Excellent Suitability – Soldering, Brazing; Fair Suitability – Oxyacetylene Welding; Poor Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding Typical uses: Emblem; Ornaments; Door Hardware for Prisons; Hardware; Ornamental Fittings; Window Hardware; Andirons; Chandeliers; Decorative Furniture Legs; Furniture; Musical Instruments; Battery Clamps; Ferrules; Gas Cocks; Mechanical Components where Looks are Important; Radiator Fittings; Valves; Marine Hardware; Ship Trimmings; Plumbing Parts Applicable Specifications: As Centrifugal Cast - Castings SAE J462, Castings ASTM B271/B271M, Castings SAE J461; As Continuous Cast – Castings SAE J461, Castings SAE J462; As Sand Cast – Castings ASTM B584, ASTM B763/B763M, Castings SAE J462, Castings SAE J461; Ingot - ASTM B30 |