MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay CEROX™ 1650 Surfactant
Categories: Fluid

Material Notes: Description: Cerox™1650 offers an optimized polishing performance for optical and ophthalmic lenses as well as for other demanding applications like photomask and glass hard disks.

Benefits: High and long lasting polishing efficiency, Very high surface quality and Quality consistency.

Features: Retains its effectiveness over a long time, even when used under demanding conditions of polishing, can be used with most types of pads, can also be used successfully in polishing wheels.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Loss On Ignition <= 1.0 %
Particle Size 1.0 - 2.0 µmD50 Sedigraph
 1.5 - 3.0 µmD50 Laser
 
Component Elements PropertiesOriginal ValueComments
CeO2 60 - 70 %
 
Descriptive Properties
Content>90%TREO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corning Pyrex® 7740 Borosilicate Glass Sheet
Quartz (SiO2)
Corning ULE® 7973 EUV Standard Grade Ultra Low Expansion Glass

WRHOD105 / 137336

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.