MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChevronTexaco 220 PMO ashless
Categories: Fluid; Lubricant

Material Notes: Texaco PMO Ashless oils deliver value through:
  • High temperature stability — Contain an effective oxidation inhibitor to protect the oil at elevated ambient operating temperatures.
  • Long lubricant life — A well-balanced additive package to minimize breakdown and extend oil life. Gives excellent performance in the FAG FE-8 Bearing Test.
  • Excellent water separability — The lubricant separates readily from water.
  • Effective foam inhibition — Reduces amount of entrained air in the oil, minimizing the possibility of pump cavitation and also prevents surface foam.
  • Pall wet filterability — Texaco PMO Ashless oils consistently provide the best wet aged filtration with low micron filters versus all other competitive paper machine oils

Texaco PMO Ashless oils are the next generation circulating oils for the pulp and paper industry.

Their ashless extreme pressure additive packages include rust, oxidation, and foam inhibitors.

Their outstanding oxidation stability minimizes deposit formation.

Their ashless formulations facilitate reclaiming and recycling of circulating oils.

They have excellent water separating ability (demulsibility), and also have superior wet filterability with fine porosity oil filters, as demonstrated by the Pall Filterability Test.

Texaco PMO Ashless oils are formulated to meet the critical demands of a circulating oil in a paper machine. This includes not only the paper machine bearings but other equipment associated with the operation such as calender stack bearings and crown control rolls. These systems expose the lubricant to a broad range of operating temperatures which hasten oxidation. The oil is constantly contaminated with water, oxidation byproducts, and other particulates. Texaco PMO Ashless oils can have a long lubricant life in spite of these contaminants and still do an outstanding job of keeping the circulating oil system clean and lubricating the many plain and antifriction bearings associated with this complex high speed equipment.

The Texaco PMO Ashless oils series is recommended for use in all circulating systems of paper machines, including wet-end systems, dryer bearings, and calender stacks.

Texaco PMO Ashless oils have been used successfully in the lubrication of many types of paper machine equipment including Valmet, Beloit, and Voith Sulzer paper machine equipment.

In addition, PMO Ashless oils exceed the best of the competition in the Pall Filterability Test using low micron filters.

Texaco PMO Ashless oils ISO 220 and 320 may also be used in plain and antifriction bearings.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 220719; MSDS Number: 8620

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 27.7 °27.7 °
Viscosity Measurement 9797Viscosity Index
Saybolt Viscosity at 100°F 1104 SUS1104 SUS
Saybolt Viscosity at 210°F 94.2 SUS94.2 SUS
Kinematic Viscosity at 40°C (104°F) 209 cSt209 cSt
Kinematic Viscosity at 100°C (212°F) 18.4 cSt18.4 cSt
Oxidative Stability 6.25 hour6.25 hourto 25 psi drop; ASTM D2272
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °F
Flash Point 249 °C480 °F
 
Descriptive Properties
FZG Pass Stage12DIN 51354
Rust PreventionPass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WTEXA129 / 77008

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.