Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combination with excellent dimensional stability, low warp and resistance to sink-mark formation. It exhibits high strength, rigidity, and good heat distortion temperature. It resists creep under load and the heat stabilizer system extends its retention of properties at elevated temperatures. It has good chemical resistance to greases, oils and hydrocarbons. |