A 30% glass reinforced polycarbonate for increased mechanical strength and thermal properties. Also available with UV stabilizer. 1433: with UV stabilizer; 1433-H2: with improved UV stabilizer. Data provided by the manufacturer |
PC; Ashley Polymers, Inc. |