MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Beijing Chemical Industry KAIFA® MN201-G30 Nylon 66 Resin
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 30% glass fiber reinforced, thermal resistant

Information provided by Beijing Chemical Industry Research Institute (Group)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 150 MPa21800 psiASTM D638
Flexural Strength 210 MPa30500 psiASTM D790
Charpy Impact Unnotched 7.50 J/cm²35.7 ft-lb/in²ISO179
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 30.0 kV/mm
@Thickness 2.00 mm
762 kV/in
@Thickness 0.0787 in
ASTM D149
Dissipation Factor 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 240 °C446 - 464 °F
Middle Barrel Temperature 265 - 270 °C509 - 518 °F
Front Barrel Temperature 265 - 270 °C509 - 518 °F
Nozzle Temperature 265 - 270 °C509 - 518 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 130 °C266 °F
Dry Time 4 hour4 hour
Injection Pressure 90.0 - 120 MPa13100 - 17400 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKAIF29 / 48611

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.