Hostacom ERC 213N C12A24 is a 15% talc filled PP copolymer, with good flowability, excellent impact/stiffness balance and excellent scratch resistance. The product is available as a customized color matched product in pellet form. This grade is delivered in C12A24 onyx black color version. This product is also available in other colors, new colors can be developed depending on customer requirements. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Instrument Panels Market: Automotive Processing Method: Injection Molding Attribute: Good UV Resistance Information provided by LyondellBasell. |