MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C42200
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability, good hot formability. Fabricated by blanking, piercing, forming and drawing.

Applications: sash chains, fuse clips, terminals, spring washers, contact springs, electrical connectors.

Available as flat products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 296 - 607 MPa42900 - 88000 psi
Tensile Strength, Yield 103 - 517 MPa14900 - 75000 psiDepending on temper
Elongation at Break 46 %46 %in 50.8 mm.
Modulus of Elasticity 110 GPa16000 ksiHard
 110 GPa16000 ksiHard
 125 GPa18100 ksiAnnealed
 125 GPa18100 ksiAnnealed
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
 30 %30 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000550 ohm-cm
@Temperature 20.0 °C
0.00000550 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 130 W/m-K
@Temperature 20.0 °C
902 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1020 - 1040 °C1870 - 1900 °F
Solidus 1020 °C1870 °F
Liquidus 1040 °C1900 °F
Annealing Point 499 - 677 °C930 - 1250 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 500 - 675 °C932 - 1250 °F
Hot-Working Temperature 830 - 890 °C1530 - 1630 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 89 - 89 %89 - 89 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.050 %<= 0.050 %
Phosphorus, P <= 0.35 %<= 0.35 %
Tin, Sn 0.80 - 1.4 %0.80 - 1.4 %
Zinc, Zn 11.4 %11.4 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C41300
Copper, UNS C42500
Copper, UNS C43500
8% Aluminum Bronze, UNS C61000
Copper, UNS C40800

MC42200b1 / 11311

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.