MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow Dow™ DMDA-8910 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow DMDA-8910 NT 7 HDPE is produced via UNIPOL™ Process Technology from Dow and is intended for use in injection molding applications including material handling and industrial container applications. The resin is designed to meet rigorous performance characteristics, including environmental stress crack resistance and impact strength, while maintaining excellent processing characteristic beneficial for molders.
Main Characteristics:
  • Injection or Compressing Molding
  • Designed for caps and closures
  • Excellent impact strength, stress crack resistance and processability
  • Very narrow molecular weight distribution
  • Excellent Organoleptic properties
Complies with: US FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.954 g/ccASTM D792
ESCR 100% Igepal® 12 hour
@Temperature 50.0 °C
F50; ASTM D1693
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59ASTM D2240
Tensile Strength at Break 2300 psiASTM D638
Tensile Strength, Yield 3500 psiASTM D638
Elongation at Break 260 %ASTM D638
Elongation at Yield 9.0 %ASTM D638
Flexural Modulus 124000 psi2% Secant; ASTM D790B
 145000 psi1% Secant; ASTM D790B
Tensile Impact Strength 59.0 ft-lb/in²Type S; ASTM D1822
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °F
Crystallization Temperature 241 °F
Deflection Temperature at 0.46 MPa (66 psi) 149 °FUnannealed; ASTM D648
Vicat Softening Point 254 °FASTM D1525
Brittleness Temperature <= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF448 / 311141

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.