MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eastman Tritan™ TXF1021 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Product Description: Eastman Tritan™ Copolyester TXF1021 is an amorphous, opaque material offering UL-94 V2 performance with outstanding aesthetics and gloss. Eastman Tritan™ Copolyester TXF1021 has many outstanding features that include excellent toughness, hydrolytic stability, heat resistance, chemical resistance, and melt flowability. Eastman Tritan™ Copolyester TXF1021 offers improved design flexibility needed in portable consumer electronic devices. Eastman Tritan™ Copolyester TXF1021 has passed FDA/ISO 10993 testing for skin sensitization. Eastman Tritan™ Copolyester TXF1021 contains a non-halogenated flame retardant.

Application/Uses:

  • Computer and Video Game accessories/peripherals
  • Personal care devices
  • Portable consumer electronic devices
  • Small appliance housings
Key Attributes:
  • Ease of decoration
  • Ease of processing
  • Ease of secondary operations
  • Excellent aesthetics and gloss
  • Excellent hydrolytic stability
  • Good chemical resistance
  • Good heat resistance
  • Good melt flowability
  • Good toughness

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 109109ASTM D785
Tensile Strength at Break 46.0 MPa6670 psiASTM D638
Tensile Strength, Yield 42.0 MPa6090 psiASTM D638
Elongation at Break 133 %133 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 1.611 GPa233.7 ksiASTM D638
Flexural Modulus 1.743 GPa252.8 ksiASTM D790
Izod Impact, Notched 4.36 J/cm8.17 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D4812
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.04
@Frequency 1e+6 Hz
3.04
@Frequency 1e+6 Hz
1.5 mm
 3.31
@Frequency 1000 Hz
3.31
@Frequency 1000 Hz
1.5 mm
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FASTM D648
Flammability, UL94  V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 282 °C500 - 540 °F
Mold Temperature 38.0 - 66.0 °C100 - 151 °F
Drying Temperature 88.0 °C190 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tritan™ MXF121 Medical Grade Copolyester
Eastman Tritan™ MX731 Medical Grade Copolyester
Eastman Tritan™ VX401 Copolyester
Avient Trilliant™ HC X THC 1100 Natural Copolyester
Avient Versaflex™ OM 2262 Thermoplastic Elastomer (TPE)

PEATM5199 / 222393

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.