MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Advanced Materials Stat-Rite® M809 Acrylic Alloy
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Product Description: M809 is a static dissipative acrylic alloy. It utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded, injection molded or thermoformed into components.
Availability: Asia Pacific, Europe, Latin America, North America
Additive: Antistatic
Features: Antistatic; Contact Clarity; ESD Protection; Humidity Resistant; Low (to None) Ion Content; Recyclable Material
Uses: Electrical/Electronic Applications; Medical Packaging; Packaging
Appearance: Translucent
Forms: Sheets
Processing Method: Extrusion; Injection Molding; Thermoforming

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Elongation at Break 30 %30 %ASTM D638
Tensile Modulus 1.45 GPa210 ksiASTM D638
Flexural Modulus 1.45 GPa210 ksiASTM D790
Izod Impact, Notched 1.39 J/cm2.60 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+10 ohm-cm4.00e+10 ohm-cmASTM D257
Surface Resistance 6.00e+9 ohm6.00e+9 ohm12% RH; ESD S11.11
 1.00e+10 ohm1.00e+10 ohm50% RH; ASTM D257
Static Decay <= 0.10 sec<= 0.10 sec1000 V to 10 V, CPM, 50% RH
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.2 °C153 °FUnannealed; ASTM D648
 
Descriptive Properties
Ionic Content15 ng/cm2Anions PO4
 15 ng/cm2Anions SO4
 20 ng/cm2Anion Cl
 200 ng/cm2Cations Na+
 4 ng/cm2Anions NO3
Outgassing15 µg/gStyrene
 180 µg/gToluene
 250 µg/gTotal Organics
 40 µg/gMMA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR6016 / 268318

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.