MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC EXTEM™ Resin VH1003P Thermoplastic Polyimide (TPI) (Europe)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003.

Features: High Heat Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D792
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.600 %0.600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.75 %1.75 %ISO 62-1
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 360 °C
8.0 cP
@Load 11.0 lb,
Temperature 680 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 15.5 g/10 min
@Load 6.60 kg,
Temperature 367 °C
15.5 g/10 min
@Load 14.6 lb,
Temperature 693 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 140 MPa20300 psiH358/30; ISO 2039-1
Tensile Strength at Break 78.0 MPa11300 psi5 mm/min; ISO 527
 96.0 MPa13900 psi5 mm/min; ASTM D638
Tensile Strength, Yield 95.0 MPa13800 psi5 mm/min; ISO 527
 96.0 MPa13900 psi5 mm/min; ASTM D638
Elongation at Break 50 %50 %5 mm/min; ASTM D638
 50 %50 %5 mm/min; ISO 527
Elongation at Yield 6.0 %6.0 %5 mm/min; ASTM D638
 8.5 %8.5 %5 mm/min; ISO 527
Tensile Modulus 3.11 GPa451 ksi1 mm/min; ISO 527
 3.51 GPa509 ksi5 mm/min; ASTM D638
Flexural Strength 123 MPa17800 psiyield, 2 mm/min; ISO 178
 155 MPa22500 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
 159 MPa23100 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.08 GPa447 ksi2 mm/min; ISO 178
 3.17 GPa460 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 69.0 J50.9 ft-lbASTM D256
 74.0 J
@Temperature -30.0 °C
54.6 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched NBNBASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Dart Drop, Total Energy 33.0 J24.3 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.41
@Frequency 1000 Hz
3.41
@Frequency 1000 Hz
ASTM D150
 3.41
@Frequency 100 Hz
3.41
@Frequency 100 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
432 kV/in
@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor  0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
IEC 60250
 0.0080
@Frequency 100 Hz
0.0080
@Frequency 100 Hz
IEC 60250
 0.025
@Frequency 50.0 - 60.0 Hz
0.025
@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  50.0 µm/m-°C
@Temperature -40.0 - 150 °C
27.8 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow  50.0 µm/m-°C
@Temperature -40.0 - 150 °C
27.8 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
Thermal Conductivity 0.220 W/m-K1.53 BTU-in/hr-ft²-°FASTM E1530
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 237 °C
@Thickness 6.40 mm
459 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 228 °C442 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 217 °C
@Thickness 3.20 mm
423 °F
@Thickness 0.126 in
unannealed; ASTM D648
 230 °C
@Thickness 6.40 mm
446 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 238 °C460 °FRate B/120; ISO 306
 242 °C468 °FRate B/50; ISO 306
 242 °C468 °FRate B/50; ASTM D1525
Oxygen Index 45 %45 %ISO 4589
Glow Wire Ignition Temperature 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
IEC 60695-2-12
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %
@Thickness 2.54 mm
2.0 %
@Thickness 0.100 in
ASTM D1003
Transmission, Visible 58 %
@Thickness 2.54 mm
58 %
@Thickness 0.100 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 375 - 400 °C707 - 752 °F
Zone 2 370 - 395 °C698 - 743 °F
Zone 3 380 - 405 °C716 - 761 °F
Melt Temperature 380 - 405 °C716 - 761 °FInjection Molding
Mold Temperature 135 - 165 °C275 - 329 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 24.0 hour24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80055 / 288002

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.