MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 512.0-F, Sand Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 512.0-F; UNS A05120; AA512.0-F; Al512.0-F
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.65 g/cc0.0957 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 35 - 6535 - 65AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 7373Estimated from Brinell Hardness.
Tensile Strength, Ultimate >= 117 MPa>= 17000 psiAA
Tensile Strength, Yield >= 68.9 MPa
@Strain 0.2 %
>= 10000 psi
@Strain 0.2 %
AA
Tensile Modulus 71.0 GPa10300 ksiEstimated
Poissons Ratio 0.330.33Estimated
Machinability 70 %70 %0-100 Scale (100=best)
Shear Modulus 26.7 GPa3870 ksiEstimated
Shear Strength 75.0 MPa10900 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000450 ohm-cm0.00000450 ohm-cmAA; Typical 38% IACS Conductivity
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 389 J/g167 BTU/lbTypical for cast aluminum
CTE, linear  22.9 µm/m-°C
@Temperature 20.0 - 100 °C
12.7 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical
 24.8 µm/m-°C
@Temperature 20.0 - 300 °C
13.8 µin/in-°F
@Temperature 68.0 - 572 °F
AA; Typical; average over range
Specific Heat Capacity 0.963 J/g-°C0.230 BTU/lb-°FTypical for cast aluminum
Thermal Conductivity 146 W/m-K1010 BTU-in/hr-ft²-°FAA; Typical at 25°C
Melting Point 588 - 632 °C1090 - 1170 °FAA; Typical
Solidus 588 °C1090 °FAA; Typical
Liquidus 632 °C1170 °FAA; Typical
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 90.9 - 95.1 %90.9 - 95.1 %As remainder
Chromium, Cr <= 0.25 %<= 0.25 %
Copper, Cu <= 0.35 %<= 0.35 %
Iron, Fe <= 0.60 %<= 0.60 %
Magnesium, Mg 3.5 - 4.5 %3.5 - 4.5 %
Manganese, Mn <= 0.80 %<= 0.80 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si 1.4 - 2.2 %1.4 - 2.2 %
Titanium, Ti <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
515.0 Aluminum Composition Spec
515.2 Aluminum Composition Spec
512.2 Aluminum Composition Spec
Aluminum 4021 Composition Spec
516.0 Aluminum Composition Spec

MAC5120F / 10126

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.