MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Toyobo Celstran® CFR-TP PP GF60-13 PP, 60% E-glass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 60% Glass Fiber Filler

Material Notes: Product Description: Celstran CFR-TP PP GF60-13 is a 60% E-glass by weight PP continuous fiber (uni-directional) reinforced thermoplastic composite tape. This material exhibits a high strength-to-weight ratio, excellent toughness and chemical resistance. It is well suited for industrial, automotive, and sporting goods applications where cost and processability are critical. The material is available in natural and black colors. Alternate tape widths and thickness maybe available.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Forms: Tape

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 106000 psiCFR-TP tape, 0°; ASTM D3039M
Elongation at Break 3.0 %CFR-TP tape, 0°; ASTM D3039M
Tensile Modulus 3.73e+6 psiCFR-TP tape, 0°; ASTM D3039M
Flexural Strength 75600 psiCFR-TP tape, 0°; ASTM D790
Flexural Modulus 3.90e+6 psiCFR-TP tape, 0°; ASTM D790
Flexural Strain at Break 2.2 %CFR-TP tape, 0°; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 343 °FISO 11357-3
Glass Transition Temp, Tg 14.0 °FISO 11357-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6221 / 310914

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.