MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron Abokote 8106-1 Water-Based Epoxy Coating for Floors
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Abokote 8106-1 is a water-based epoxy coating that is part of the Abokote 8106-1 Flooring System which consists of this water-based epoxy coating, vinyl color chips, and Abokote 57-1 clear acrylic top-coat. The Flooring System is recommended for floors requiring a durable, water-resistant, attractive coating with low odor. This system has the attributes of solvent-based epoxy systems without solvent vapors. For this reason it can be used in areas without strong ventilation such as utility rooms, basements, and other confined spaces. It comes in many color options allowing it to be used in locations where an aesthetically pleasing flooring system supporting heavy foot traffic is needed. Features: high bond strength, water-resistant, low odor and no solvents, slip resistant, unlimited standard and custom colors, abrasion resistant, and glossy. Benefits: high durability, easy installation, low hazard for installation, easy maintenance, design options, and cost-effective.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content 257.6 g/lEPA method #24
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 298 psiASTM-D4541
Coefficient of Friction 1.3Slip resistance; ASTM-D1894
 
Thermal PropertiesOriginal ValueComments
Flash Point 212 °FASTM-D3278
 
Descriptive Properties
Abrasive Resistance (g)0.101ASTM-D4060; CS 17/Load 1000/Cycles 1000
Chemical ResistanceGoodASTM-D543
Hardening Time (min)120
Hardness, pencilHBASTM-D3363
Impact Resistance22.5ASTM-D4226
Induction Period (min)30-45

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PABC839 / 107823

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.