MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Germanium Mullite, 3Al2O3-2GeO2
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 11201120kg/mm²
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.80 µm/m-°C
@Temperature 20.0 °C
3.22 µin/in-°F
@Temperature 68.0 °F
Melting Point 1550 °C2820 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.6641.664
IR Transmittance 70 %
@Thickness 0.760 mm
70 %
@Thickness 0.0299 in
cutoff is 5.3 µm.
 
Processing PropertiesMetricEnglishComments
Sintering Temperature 1500 °C2730 °FReports of sintering in a bed of GeO2 to avoid loss of GeO2.

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mullite, 3Al2O3-2SiO2
Yttria Stabilized Zirconia, YSZ
Fused Quartz
Zirconium Oxide, Zirconia, ZrO2
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3

BMULL1 / 251

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.