Description: TIPOLEN FB 243-55 is a film grade of low density polyethylene with good molten stability and excellent processability. The films made of this grade have good mechanical properties. The grade contains slip and antiblocking agents. Applications: TIPOLEN FB 243-55 is intended for carrier bags, household films, packaging films. Recommended film thickness is 0.025 to 0.08 mm. (1) Density, Vicat Softening Temperature and Shore D Hardness have been measured on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291). (2) Properties on film in M.D./T.D. - thickness of 0.07 mm (MFR=0.3 g/10min) and 0.04 mm (MFR more than 0.3 g/10min), blow up ratio 2:1. Information provided by Molgroup Chemicals |