MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Materia Proxima® HTI 1400 Polydicyclopentadiene Thermoset Resin
Categories: Polymer; Thermoset; Polydicyclopentadiene (PDCPD)

Material Notes: Materia Proxima HTI 1400 is an olefin thermoset resin designed to provide thermal insulation for temperatures up to 400°F (204°C). Proxima HTI 1400 is particularly suitable for use for subsea thermal insulation for projects in ultra-deep water applications.

Information provided by Materia, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccPolymer; ASTM D792
Water Absorption <= 0.20 %
@Temperature 100 °C
ASTM D570
Brookfield Viscosity 5.0 cP
@Temperature 30.0 °C
Resin
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 74ASTM D2240
Tensile Strength, Yield 35.0 MPaASTM D638
Elongation at Break >= 75 %ASTM D638
Elongation at Yield 6.8 %ASTM D638
Tensile Modulus 1.40 GPaASTM D638
Compressive Strength 35.0 MPaASTM D695
Compressive Modulus 1.115 MPaASTM D695
Izod Impact, Notched 1.80 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.175 W/m-KASTM C518
Maximum Service Temperature, Air 204 °C
Glass Transition Temp, Tg 52.0 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMATERI992 / 265397

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.