Product Description: HD 9830.02 is a blow molding grade high density polyethylene copolymer with a bimodal molecular weight distribution. It provides a very good balance of stress crack resistance, stiffness and impact strength with excellent processability due to its next generation branched structure. Availability: Latin America, North America and South America Additive: - Thermal Stabilizer: Yes
- Antistatic: No
- UV Stabilizer: No
Applications: - Blow Molding
- Drainage Pipes
- Personal Care
- Sheet Extrusion
Information provided by ExxonMobil |