MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Escorene™ FL 00309 Ethylene Vinyl Acetate Copolymer (European Grade)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: FL 00309 is a copolymer of ethylene and vinyl acetate.
Processing Conditions: Processing temperatures above 270°C (513°F) may cause resin degradation.

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Cast Film
  • Co-Extrusion Films
  • Food packaging
  • Injection Molding
  • Lamination Film

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.929 g/cc0.0336 lb/in³ExxonMobil method
Vinyl Acetate Content 9.4 %9.4 %ExxonMobil method
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 93
@Time 15.0 sec
93
@Time 0.00417 hour
Molded Properties; ISO 868
Tensile Strength at Break >= 0.689 MPa>= 100 psiMolded Properties; ISO 527-2/1A/100
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 600 %600 %ASTM D882
Tensile Modulus 0.0758 GPa11.0 ksiMolded Properties; ISO 527-2/1
Elmendorf Tear Strength MD 80 g80 gASTM D1922
Elmendorf Tear Strength TD 130 g130 gASTM D1922
Dart Drop Test 360 g0.794 lbASTM D1709A
Film Tensile Strength at Break, MD 24.8 MPa3600 psiASTM D882
Film Tensile Strength at Break, TD 24.1 MPa3500 psiASTM D882
1% Secant Modulus, MD 103 MPa15000 psiASTM D882
1% Secant Modulus, TD 110 MPa16000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 96.1 °C<= 205 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 74.4 °C166 °FASTM D1525
 
Descriptive Properties
Blending Temperature270

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Escorene™ UL 00218CC3 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ AD 0633EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ FL 00714 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ FL 02020 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ UL 00119 Ethylene Vinyl Acetate Copolymer (European Grade)

PEX99091 / 175327

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.