MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ChevronTexaco Capella® P 68
Categories: Fluid; Lubricant

Material Notes: Texaco Capella P 68 delivers value through:
  • Reduced oil carryover — Low volatility and greater ammonia immiscibility result in significantly less oil reaching the evaporator, increasing refrigeration efficiency and reducing maintenance. The low pour point and high viscosity index insures that any oil which does reach the evaporator will drain more rapidly than a naphthenic oil.
  • Reduced sludging and formation of harmful deposits in the high temperature environment of the compressor. As a result, equipment life and lubricant life can be extended while reducing maintenance.
  • Stable viscosity — Base stock properties allow the oil to maintain a stable viscosity, staying in grade longer than a naphthenic refrigeration oil.
  • Maximum protection for critical parts of the compressor provided by high viscosity index, low foaming tendency, and inherent antiwear properties. The oil maximizes equipment life and life to overhaul by providing superior lubrication to all moving parts.
  • Extended drain intervals — Resistance to thermal degradation allows customers to extend drain intervals.
  • Less make-up oil required — Significantly less make-up oil is required because this product resists "carryover" to the refrigeration systems low temperature side.

Texaco Capella P 68 provides superior wear protection for reciprocating, vane, and screw compressors.

Texaco Capella P 68, formulated with Group II base stocks, is designed to specifically address the requirements of ammonia refrigeration systems and provide better results than naphthenic refrigeration oils in these systems. Texaco Capella P 68 provides advantages over naphthenic refrigeration oils in the critical performance areas of lubrication, thermal stability, and reduction of oil carryover

Texaco Capella P 68 is the lubricant of choice for rotary screw, reciprocating, or rotary vane compressors in ammonia refrigeration systems. The single ISO grade is consistent with the recommendation of equipment manufacturers.

Although designed for use in ammonia refrigeration systems, Texaco Capella P 68 is also recommended for use in systems using refrigerant R-22 and R-502 provided the evaporator temperature is above -32°C (-25°F). It is not recommended for systems using refrigerant R-12 or R-134a.

Texaco Capella P 68 is compatible with the seal elastomers commonly used in refrigeration compressors (e.g., Buna-N, chloroprene). Naphthenic refrigeration oils can compromise the integrity of certain seal elastomers. It is good maintenance practice to install new seal elastomers when replacing a naphthenic refrigeration oil. This is especially important when chloroprene (neoprene) seals are present. Texaco Capella P 68

  • meets the requirements of the U.S. Department of Agriculture (ASDA) for use in federally inspected meat and poultry plants as an H2 lubricant where no food contact will occur.
  • meets the requirements of NSF International as an H2 lubricant for use in federally inspected meat and poulty plants where there is no possibility of food contact.

Texaco Capella P 68 is recommended for use in Vilter and Sabroe refrigeration compressors.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222696; MSDS Number: 8703

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 31.8 °31.8 °
Viscosity Measurement 102102Viscosity Index
Saybolt Viscosity at 100°F 335 SUS335 SUS
Saybolt Viscosity at 210°F 54 SUS54 SUS
Kinematic Viscosity at 40°C (104°F) 64.6 cSt64.6 cSt
Kinematic Viscosity at 100°C (212°F) 8.5 cSt8.5 cSt
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
889 kV/in
@Thickness 0.0394 in
 
Thermal PropertiesMetricEnglishComments
Pour Point -38.0 °C-36.4 °F
Flash Point 244 °C471 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Process Technologies Inc BUNA-N/Metal - Metal Detectable Sanitary Gasket
Process Technologies Inc BUNA-N Sanitary Gasket
Freudenberg N470 Hydrocarbon Elastomer Nitrile
ChevronTexaco ISO 68 Ammonia Refrigeration Oil

WTEXA035 / 76914

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.