MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LKAB Minerals FireCarb TEG-315 Expandable Graphite
Categories: Carbon; Graphite; Other Engineering Material; Additive/Filler for Polymer

Material Notes: High quality crystalline flake graphite that has a medium to high source of carbon, typically 80 – 99%

Expandable graphite belongs to a group of products called "intumescents." The primary property of intumescents is their ability to expand when heated. On exposure to heat, the retained solutions within FireCarb produce a gas that expands and forces open the graphite platelets. The expansion that expandable graphite offers (up to 350 x volume at 1000°C) makes it more effective than conventional intumescents. This expansion has the added benefit of creating high pressure, especially when mechanically restricted, and at the same time an insulating carbonaceous char is formed which protects the substructure from the heat source. Typically expansion starts at 170°C, however delayed expansion products can be manufactured to the customers specification. Applications: Passive Fire Protection, Intumescent Coatings, Bituminous Roofing Systems, Plastic & Rubber Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 12 %
Water Absorption at Saturation <= 1.0 %
Particle Mesh Size >= 80 Mesh80%; ASTM E11-87
pH 5.0 - 7.0
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 95 %
 
Descriptive Properties
AppearanceBlack flakes
Expansion, ml/gm2201000°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoorsTek CRB-100 Resin-Impregnated Carbon Graphite
Graphite, Carbon, C
NeoGraf eGRAF® HITHERM™ HT-705 Graphite
NeoGraf eGRAF® HITHERM™ HT-720 Graphite
NeoGraf eGRAF® SPREADERSHIELD™ SS1500 Graphite

CMINEL02 / 1567

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.