MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ STAT-KON™ Compound DEF13 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DEF13 compound is based on Polycarbonate (PC) resin containing 5% glass fiber and 15% carbon fiber. Added features of this grade include: Electrically Conductive.

Features: High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Density 1.29 g/cc0.0466 lb/in³ASTM D792
 1.29 g/cc0.0466 lb/in³ISO 1183
Water Absorption 0.070 %
@Time 86400 sec
0.070 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 12.0 MPa1740 psi5 mm/min; ISO 527
 118 MPa17100 psiASTM D638
Tensile Strength, Yield 44.0 MPa6380 psi5 mm/min; ISO 527
 61.0 MPa8850 psi5 mm/min; ASTM D638
Elongation at Break 1.9 %1.9 %5 mm/min; ISO 527
 4.0 %4.0 %ASTM D638
Tensile Modulus 12.41 GPa1800 ksi1 mm/min; ISO 527
 17.87 GPa2592 ksi50 mm/min; ASTM D638
Flexural Strength 159 MPa23100 psi1.3 mm/min, 50 mm span; ASTM D790
 211 MPa30600 psi2 mm/min; ISO 178
Flexural Modulus 9.44 GPa1370 ksiASTM D790
 18.5 GPa2680 ksi2 mm/min; ISO 178
Izod Impact Notched 101 J74.5 ft-lbASTM D256
Izod Impact, Unnotched 5.13 J/cm
@Thickness 6.40 mm
9.61 ft-lb/in
@Thickness 0.252 in
ASTM D4812
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²80*10*4; ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 - 1.00e+6 ohm100 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 148 °C298 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 147 °C
@Thickness 3.20 mm
297 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 144 °C291 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 144 °C
@Thickness 3.20 mm
291 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94  V-1
@Thickness >=1.50 mm
V-1
@Thickness >=0.0591 in
UL 94
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81221 / 289168

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.