MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ THERMOCOMP™ Compound DF0069P Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP DF0069P compound is based on Polycarbonate (PC) resin containing 30% glass fiber. Added features of this grade include: Exceptional Processing. Flame Retardant.

Features: High Stiffness,Flame Retardant,Exceptional Processing,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ASTM D792
 1.46 g/cc0.0527 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.0900 %0.0900 %23°C/50% RH/24 hrs; ASTM D570
 0.120 %0.120 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 119 MPa17300 psi5 mm/min; ISO 527
 127 MPa18400 psi5 mm/min; ASTM D638
Elongation at Break 2.0 %2.0 %5 mm/min; ISO 527
 2.6 %2.6 %5 mm/min; ASTM D638
Tensile Modulus 9.10 GPa1320 ksi1 mm/min; ISO 527
 9.71 GPa1410 ksi50 mm/min; ASTM D638
Flexural Strength 196 MPa28400 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 8.48 GPa1230 ksi2 mm/min; ISO 178
 9.02 GPa1310 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 107 J78.9 ft-lbASTM D256
Izod Impact, Unnotched 7.55 J/cm14.1 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 48.0 kJ/m²22.8 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 9.00 J6.64 ft-lbASTM D3763
Impact Test 2.00 J1.48 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 27.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 45.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
25.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 139 °C
@Thickness 3.20 mm
282 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 136 °C277 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 135 °C
@Thickness 3.20 mm
275 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81527 / 289474

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.