MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Lanxess Addolink® 1604 Crosslinking Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Addolink 1604, an aromatic diamine, is used as a crosslinking agent in combination with prepolymers for the manufacture of high-quality heat curing PUR elastomers, giving considerably longer casting times than other amine crosslinking agents.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.132 g/cc
@Temperature 110 °C
0.04090 lb/in³
@Temperature 230 °F
 1.14 g/cc
@Temperature 100 °C
0.0412 lb/in³
@Temperature 212 °F
 1.148 g/cc
@Temperature 90.0 °C
0.04147 lb/in³
@Temperature 194 °F
Water Absorption <= 0.15 %<= 0.15 %
Viscosity  12 cP
@Temperature 110 °C
12 cP
@Temperature 230 °F
 19 cP
@Temperature 100 °C
19 cP
@Temperature 212 °F
 27 cP
@Temperature 90.0 °C
27 cP
@Temperature 194 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 86.0 - 94.0 °C187 - 201 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature <=30.0 °C
12.0 Month
@Temperature <=86.0 °F
 
Descriptive Properties
Appearanceyellow or brown granules
Specifications117-124Average equivalent weight (on amine) RC-method A0192:

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8203 / 208596

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.