MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Huafon JF-P-5265AC/JF-I-5218 Polyester
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: Characteristics: Medium hardness, low temperature resistance.

Applications: For man/woman shoes

Information provided by Zhejiang Haufon New Materials Corp., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.300 - 0.350 g/cc0.0108 - 0.0126 lb/in³Free rise foam density
 0.550 - 0.600 g/cc0.0199 - 0.0217 lb/in³Molded
 1.15 - 1.17 g/cc
@Temperature 40.0 °C
0.0415 - 0.0423 lb/in³
@Temperature 104 °F
JF-P-5265AC
 1.18 - 1.20 g/cc
@Temperature 40.0 °C
0.0426 - 0.0434 lb/in³
@Temperature 104 °F
JF-P-5218
Viscosity  400 - 700 cP
@Temperature 40.0 °C
400 - 700 cP
@Temperature 104 °F
JF-P-5218
 1500 - 2400 cP
@Temperature 40.0 °C
1500 - 2400 cP
@Temperature 104 °F
JF-P-5265AC
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 6.00 MPa>= 870 psi
Elongation at Break >= 500 %>= 500 %
Tear Strength >= 25.0 kN/m>= 143 pli
Abrasion >= 25>= 25[%] NBS abrasion resistance
 
Processing PropertiesMetricEnglishComments
Mold Temperature 45.0 - 55.0 °C113 - 131 °F
 
Descriptive Properties
AppearanceLiquid or waxy40°C, JF-P-5265AC
 Transparent and pure liquid40°C, JF-I-5218
Asker A Hardness48-55
Asker C Hardness65-70
Cream time7-10 sec
Demold time5-7 min
Flexing resistanceNo crack-30°C, Breakage length
Material Temperature38-42°C
P+C/l Mix ratio100/80-81
Rise time30-40 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUAF029 / 294972

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.