MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mallard Creek Polymers Rovene® 6112 Styrene-Acrylic Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Rovene® 6112 is a hard, film forming, low glycol ether and VOC vehicle with a moderately low glass transition temperature for flexographic and gravure inks and overprint varnishes. Rovene® 6112 exhibits good water and grease resistance. This polymer allows formulating for film integrity and flexibility without adversely affecting the blocking resistance of the inks and overprint varnishes. Inks and overprint varnishes formulated with Rovene® 6112 can be easily formulated with graphic arts industry standard products and additives.

Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6112 Material Safety Data Sheet before handling, storing, or using this product.

Information provided by Mallard Creek Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.70 lb/gal
Solids Content 45 - 47 %
pH 8.1 - 8.8
Brookfield Viscosity <= 1000 cP#20/200
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 50[mgKOH/g]
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 20.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mallard Creek Polymers Rovene® 6104 Styrene-Acrylic Emulsion
Mallard Creek Polymers Rovene® 6126 Styrene-Acrylic Emulsion
Mallard Creek Polymers Rovene® 6119 Styrene-Acrylic Emulsion
Mallard Creek Polymers Rovene® 6117 Acrylic Emulsion
Mallard Creek Polymers Rovene® 6111 Styrene-Acrylic Emulsion

PMCP130 / 157407

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.