MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Danquinsa DANTHANE® 125KB TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: DANTHANE_ 125KB is a polyester based, aromatic TPU, already colored in blue. This TPU granule is best suitable for coatings and films, that must show high flexibility also at low temperatures. DANTHANE_ 125KB is mainly used at the production of blue colored transport elements (transport and conveyor belt coatings).

Application: DANTHANE_ 125KB is applied at the hot melt coating of industrial textiles. The coated textiles are used for transport and drive sections. DANTHANE_ 125KB is favored used for sinter coatings of textiles. Concerning powder we refer to the type DANTHANE_ 125KB-Powder.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³DIN 53.479
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585DIN 53.505
Tensile Strength 25.0 MPa3630 psiDIN 53.504
Elongation at Break 610 %610 %DIN 53.504
100% Modulus 5.50 MPa798 psiDIN 53.504
200% Modulus 6.00 MPa870 psiDIN 53.504
300% Modulus 8.50 MPa1230 psiDIN 53.504
Abrasion 3030[mm³]; DIN 53.516
Compression Set  30 %
@Temperature 23.0 °C,
Time 252000 sec
30 %
@Temperature 73.4 °F,
Time 70.0 hour
DIN 53.517
 80 %
@Temperature 70.0 °C,
Time 86400 sec
80 %
@Temperature 158 °F,
Time 24.0 hour
DIN 53.517
 
Thermal PropertiesMetricEnglishComments
Melting Point 135 - 145 °C275 - 293 °FKofler
Softening Point 120 - 125 °C248 - 257 °FKofler
Glass Transition Temp, Tg -29.0 °C-20.2 °FDSC; DIN 51.007
 
Processing PropertiesMetricEnglishComments
Drying Temperature 90.0 - 100 °C194 - 212 °F
Dry Time 2.00 hour2.00 hour
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AspectBlue colored pearl granulecolor RAL 5015

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ139 / 294559

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.