Moplen HP500N B is a homopolymer used for general purpose injection molding applications. It exhibits good flow and stiffness. Moplen HP500N B is suitable for food contact. Availability: Asia-Pacific Application: Furniture; Housewares Market: Compounding; Consumer Products; Rigid Packaging Processing Method: Compounding; Injection Molding Attribute: Medium Flow; Medium Stiffness Information provided by LyondellBasell. |