MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Solvay DAPCO™ 3042 Fast Curing Paste Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: DAPCO™ 3042 fast curing paste adhesive is a two-part, room temperature curing, epoxy-based, 100% solids, self-extinguishing, composite edge filling and insert potting material. The material has a convenient one-to-one mix ratio by volume. The product is available in a variety of kit sizes including 50 ml, 200 mil and 400 ml side-by-side cartridges.

Features & Benefits:

  • Thixotropic flow properties
  • 100% solids content
  • Room temperature cure
  • Room temperature storage
  • 180°F (82°C) performance
  • Meets FAR 25.853
  • Fast cure rate allowing quicker production
Applications: DAPCO 3011 is commonly used for potting, stiffening and edge filling of honeycomb core.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³Part B
 1.10 g/cc0.0397 lb/in³Mixed
 1.15 g/cc0.0415 lb/in³Part A
Solids Content 100 %100 %Part A
 100 %100 %Part B
 100 %100 %Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70 - 8070 - 80
Tensile Strength 24.1 MPa3500 psi
Elongation at Break 13 %13 %
Compressive Strength  3.45 MPa
@Temperature 177 °C
500 psi
@Temperature 351 °F
 8.96 MPa
@Temperature 82.0 °C
1300 psi
@Temperature 180 °F
 55.2 MPa
@Temperature 25.0 °C
8000 psi
@Temperature 77.0 °F
Adhesive Bond Strength 13.8 MPa2000 psiShear to Aluminum (2024 T3)
Peel Strength 1.93 kN/m11.0 pliT-Peel; ASTM D1876
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthPart A
 12.0 Month12.0 MonthPart B
 
Descriptive Properties
ColorWhitePart A
 WhitePart B
 WhiteMixed
Insert pull-out strength350 psiNAS 1836-7
 590 psiNAS 1836-14
 700 psiNAS 1836-22

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCYTED021 / 180323

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.