MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik 0C404 Strip Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Special-Purpose Steel

Material Notes: Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 670 MPaannealed
 1050 MPacold rolled
 40.0 MPa
@Temperature 900 °C
 580 MPa
@Temperature 200 °C
Tensile Strength, Yield 510 MPa
@Strain 0.2 %
annealed
 1000 MPa
@Strain 0.2 %
cold rolled
 20.0 MPa
@Strain 2 %,
Temperature 900 °C
 325 MPa
@Strain 2 %,
Temperature 200 °C
Elongation at Break <= 1.0 %cold rolled
 >= 15 %annealed
 25 %
@Temperature 200 °C
 150 %
@Temperature 900 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000138 ohm-cm
@Temperature 20.0 °C
 0.000140 ohm-cm
@Temperature 400 °C
 0.000146 ohm-cm
@Temperature 800 °C
Curie Temperature 556 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.7 µm/m-°C
@Temperature 20.0 - 100 °C
 12.1 µm/m-°C
@Temperature 20.0 - 200 °C
 13.3 µm/m-°C
@Temperature 20.0 - 600 °C
 15.8 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.481 J/g-°C
@Temperature 20.0 °C
 0.663 J/g-°C
@Temperature 400 °C
 0.715 J/g-°C
@Temperature 800 °C
Thermal Conductivity 11.7 W/m-K
@Temperature 20.0 °C
 22.9 W/m-K
@Temperature 800 °C
Melting Point 1470 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.5 %
Carbon, C <= 0.020 %
Chromium, Cr 20.5 %
Iron, Fe 73.1 - 74 %As Balance
Manganese, Mn <= 0.35 %
Phosphorus, P <= 0.020 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chosun Refractories C40 Special High-Density Gunning Castable
Gray Cast Iron, ASTM A 48 Class 40
39NiCrMo3 Steel
304 Stainless Steel
AISI 1040 Steel, normalized at 900°C (1650°F), air cooled, 13 mm (0.5 in.) round

NSANDV275 / 19169

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.