MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Prime Polymer ULTZEX® 20200J LLDPE, Injection Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Advantages: Stress Cracking Resistance; Flowability

Major Applications: Cap; Daily Necessities; Industrial Parts

Information provided by Prime Polymer Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³JIS K7112
Environmental Stress Crack Resistance 8.0 hour8.0 hourASTM D1693
Melt Flow 19 g/10 min19 g/10 minJIS K7210
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5252JIS K7215
Tensile Strength, Yield 9.00 MPa1310 psiJIS K7161
Elongation at Break >= 500 %>= 500 %Nominal; JIS K7161
Modulus of Elasticity 0.190 GPa27.6 ksiJIS K7171
Charpy Impact, Notched 6.70 J/cm²31.9 ft-lb/in²JIS K7111
 
Thermal PropertiesMetricEnglishComments
Melting Point 124 °C255 °FJIS K7121
Vicat Softening Point 91.0 °C196 °FJIS K7206

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRIME032 / 313425

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.