MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

LyondellBasell Metocene HM648T Polypropylene, Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Metocene HM648T is a metallocene-catalyzed polymer for thin wall injection molding. It is nucleated and contains an antistatic agent. Metocene HM648T has an excellent stiffness and transparency, outstanding organoleptic properties and a low warpage. The main applications of Metocene HM648T are food packaging requiring low odor and low taste, cups, lids, closures and other thin wall applications. This grade is not intended for medical and pharmaceutical applications. This grade is supported for use in drinking water applications.

Availability: Africa-Middle East; Europe

Application: Housewares; TWIM Food Containers; TWIM Non-food Containers

Market: Rigid Packaging

Processing Method: Injection Molding

Attribute: Contains Antistat; Good Stiffness; High Flow; Nucleated

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 60.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
60.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psiISO 527-1, -2
Elongation at Break >= 50.0 %>= 50.0 %ISO 527-1, -2
Elongation at Yield 7.00 %7.00 %ISO 527-1, -2
Tensile Modulus 1.70 GPa247 ksiISO 527-1, -2
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FUnannealed; ISO 75B-1, -2
Vicat Softening Point 140 °C284 °FA50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 7.00 %
@Thickness 0.00100 mm
7.00 %
@Thickness 0.0000394 in
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9652 / 324587

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.