MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kraton® G1643 V Linear Triblock Copolymer
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Kraton G1643 V is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 20%. It is supplied from Taiwan. Kraton G1643 V is used in compound formulations and as a modifier of thermoplastics. It may also find use in formulating adhesives, sealants, coatings and modified bitumens.

Kraton G1643 VS - is supplied as a dusted, dense pellet.

Information provided by Kraton Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D792
Viscosity Measure 210 cSt
@Temperature 25.0 °C
25%w toluene solution; BAM 922
Melt Flow 14 - 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Ash 0.020 - 0.12 %Silica; AGAM 908
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 52
@Time 30.0 sec
ASTM D2240
Tensile Strength >= 1500 psiASTM D412
Elongation at Break >= 600 %ASTM D412
 
Descriptive Properties
Antioxidant0.06 to .14Test Method KM 08. Non-staining phenolic antioxidant.
Polystyrene Content (%m)16.6 to 20.6Test Method KM 03
Styrene / Rubber Ratio20/80
Total Extractables<=1 %mTest Method KM 05
Volatile Matter (%m)<= 1KM 04

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKQZ9007 / 239872

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.