MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon I51576R015 Silicone Rubber/Fiberglass/Alloy Laminate
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Top layer of side 2: alloy 600 foil; Bottom layer of side 2: cured silicone rubber; Substrate is 7628 fiberglass; Side 1: cured silicone rubber

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccsilicone property (alloy 600 = 8.41 g/cc); Arlon SQA-TMS-024
Thickness 1.00 millaminated foil; Arlon SQA-TMS-003
 2.00 milside 1; Arlon SQA-TMS-003
 5.50 milside 2; Arlon SQA-TMS-003
 8.00 milsubstrate; Arlon SQA-TMS-003
 16.5 miloverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45silicone property; ASTM D2240
Tensile Strength, Ultimate 900 psisilicone property; ASTM D412
Elongation at Break 400 %silicone property; ASTM D412
Adhesive Bond Strength 7.00 psibond to alloy 600; ASTM D624
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 400 V/milsilicone property; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.9 µm/m-°C
@Temperature 20.0 °C
alloy 600 property
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -70.0 °F
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 204 °C
Shelf Life 12.0 Month
@Temperature 21.1 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate
Rogers Arlon CP-375CR Silicone Rubber
Rogers Arlon 55946C028 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 55106R028 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 51106R015 Silicone Rubber/Fiberglass Laminate

PARL061 / 79713

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.