Data provided by Von Roll Isola USA. Flash Point: 24°C. Average solids: 92.5%. Usage Notes: Clear epoxy insulating varnish which penetrates and saturates extremely well, giving outstanding moisture resistance and bond strength. |
Von Roll Isola USA; Insulating Materials Incorporated |