HM4560UA-C is an UV light stabilized, pelleted high molecular weight, high density polyethylene Hexene-1 resin for medium-large blow molding. Applications: Intermediate bulk containers, agricultural containers, industrial chemical containers and pallets. Advantages: Excellent stress crack resistance, excellent resistance to most chemicals and outstanding rigidity with high impact strength and high melt strength. Information provided by Lotte Advanced Materials. |