MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sika Sikaflex® -15 LM High-performance, low-modulus elastomeric sealant
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Sikaflex-15 LM is a low-modulus, high-performance, 1-component, polyurethane-based, non-sag elastomeric sealant. Meets Federal Specification TT-S-00230C, Type II, Class A; ASTM C-920, Type S, Grade NS, Class 100/50, use T, NT, G, A, O, M; Federal Specification for silicones - TT-S-001543 A, Type non-sag. Tested in accordance with ASTM C-1382 for use in EIFS systems.

Where to use:

  • Excellent for moving joints in vertical applications.
  • Suitable for use between similar as well as dissimilar materials.
  • Typical applications include joints in concrete panel and wall systems, around window and door frames, reglets, flashing, common roofing detail applications, etc.
  • Exceptional sealant choice for high-rise and facade applications where high movement capability is required.
  • 2- and 3-hour UL Fire Rated Joint System Nos. FF-S-0007, FF-S-0037, FW-S-0015, FW-S-0018, HW-S- 0076, HW-S-0095, WW-S-0011 and WW-S-0060.
  • An effective sealant for use in Exterior Insulation Finish Systems (EIFS).
Advantages:
  • Low modulus of elasticity.
  • Easy and ready to use.
  • Eliminates time, effort, waste, and equipment clean-up.
  • Cures to a durable, flexible consistency.
  • Exceptional cut and tear resistance.
  • Stress relaxation properties.
  • Excellent adhesion.
  • Bonds to most construction materials without a primer.
  • Paintable with water-, oil- and rubber based paints.
  • Excellent resistance to aging, weathering.
  • Jet fuel resistant.
  • Proven in tough climates around the world.
  • Non-leaching.
  • Capable of +100% / -50% joint movement.
Colors include White, Colonial White, Aluminum Gray, Limestone, Black, Dark Bronze, Capitol Tan, Off-White, Beige, Almond, Coping Stone, Aluminum Stone, Medium Bronze, Redwood Tan, Hartford Green and Stone.

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20 - 3021 day; ASTM D2240
Tensile Strength 125 psi21 day; ASTM D412
Tensile Stress at Strain 50.0 psi
@Strain 100 %
ASTM D412
Elongation at Break 700 %ASTM D412
Peel Strength 25.0 pliConcrete, 0% Adhesion loss; TT-S-00230C
 25.0 pliAluminum, 0% Adhesion loss; TT-S-00230C
 25.0 pliGlass, 0% Adhesion loss; TT-S-00230C, ASTM C-794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 170 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 168 - 240 hourFinal cure
Tack-Free Time 3.00 hourTack-free touch
 2.00 - 6.00 hour
Shelf Life 6.00 Month
@Temperature 4.00 - 35.0 °C
5 gal. pails
 6.00 Month
@Temperature 4.00 - 35.0 °C
55 gal. drums
 12.0 Month
@Temperature 4.00 - 35.0 °C
10.1 fl. oz. cartridges
 12.0 Month
@Temperature 4.00 - 35.0 °C
20 fl. oz. uni-pac sausages

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIKA935 / 209842

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.