MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Envalior Durethan® BKV 215 H3.0 000000 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: PA 6-Copolymer, 15% glass fibers, injection molding, improved impact strength, heat-aging stabilized

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³ISO 60
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.0 %2.0 %50% RH; ISO 62
Water Absorption at Saturation 7.0 %7.0 %ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/in150x105x3; 280 °C / MT 80 °C; 400 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0083 cm/cm0.0083 in/in150x105x3; 280 °C / MT 80 °C; 400 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psi5 mm/min; ISO 527-1,-2
Elongation at Break 4.5 %4.5 %5 mm/min; ISO 527-1,-2
Tensile Modulus 4.50 GPa653 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 135 MPa19600 psi2 mm/min; ISO 178-A
Flexural Yield Strength 125 MPa
@Strain 3.5 %
18100 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 4.20 GPa609 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 5.5 %5.5 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 20.0 kJ/m²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  60.0 kJ/m²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
 65.0 kJ/m²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
Charpy Impact Unnotched  7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
 8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
22.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 170 µm/m-°C
@Temperature 23.0 - 55.0 °C
94.4 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 214 °C417 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 175 °C347 °FISO 75-1,-2
Vicat Softening Point 200 °C
@Load 5.10 kg
392 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Oxygen Index 22 %22 %Method A; ISO 4589-2
Shrinkage, MD 0.050 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.050 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction 150x105x3; ISO 294-4
Shrinkage, TD 0.15 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.15 %
@Treatment Temp. 248 °F,
Time 4.00 hour
150x105x3; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
 280 °C536 °Finjection molding
Mold Temperature 80.0 °C176 °Finjection molding
 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 6.00 hour2.00 - 6.00 hour
Moisture Content 0.030 - 0.12 %0.030 - 0.12 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANW9356 / 208175

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.