MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound  (discontinued **)
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled; Filled/Reinforced Thermoset

Material Notes:

Data provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.82 g/cc
Apparent Bulk Density 0.300 g/cc
Water Absorption 0.30 %48 hrs, 50°C
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cmtypical.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 41.0 - 55.0 MPa
Flexural Strength 103 MPa
Compressive Strength 186 MPa
Izod Impact, Notched 2.40 J/cm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+17 ohm-cm
Surface Resistance >= 1.00e+17 ohm
Dielectric Constant 4.0
@Frequency 1e+6 Hz
Wet
 4.1
@Frequency 1000 Hz
Wet
Dielectric Strength 14.0 kV/mmWet, Step by Step
Dissipation Factor 0.010
@Frequency 1000 Hz
Wet
 0.017
@Frequency 1e+6 Hz
Wet
Arc Resistance 160 sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 24.0 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 260 °CHeat Distortion temperature
Flammability, UL94 V-0
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 135 - 165 °CMolding temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
IDI Composites Rosite® 3550F BMC Thermoset Polyester, 30% Glass Reinforced
Emerald Performance Materials EPALLOY® 8330 A85 Epoxy Phenol Novolac Solution
Elantas EN-8 (Conap) Casting, Potting, and Molding Compound
Cosmic Plastics E4905 Mineral Filled Epoxy Molding Compound, Encapsulated Grade
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade

PAESCC / 22935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.