MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: ALATHON H4250 is a high-flow “freezer” grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic properties. Typical applications are rigid food containers such as four, five and six-quart ice cream containers that are produced at high speeds in fast cycling multi-cavity stack molds.

Regulatory Status: H4250 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.593 - 0.625 g/cc0.0214 - 0.0226 lb/in³ASTM D1895
Density 0.942 g/cc0.0340 lb/in³ASTM D1505
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 43.7 cm17.2 inEquistar test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ASTM D2240
Tensile Strength at Break 21.1 MPa3060 psi50 mm/min; ASTM D638
Elongation at Break 12 %12 %50 mm/min; ASTM D638
Tensile Modulus 0.6922 GPa100.4 ksi1% Secant; 50mm/min; ASTM D638
 0.9425 GPa136.7 ksi50mm/min; ASTM D638
Flexural Modulus 0.9411 GPa136.5 ksi12.5 mm/min; ASTM D790
 0.7040 GPa
@Strain 2 %
102.1 ksi
@Strain 2 %
Secant; 12.5 mm/min; ASTM D790
Flexural Modulus, 1% Secant 826.0 MPa119800 psi2.5 mm/min; ASTM D790
Izod Impact, Notched 0.347 J/cm0.650 ft-lb/inASTM D256
 NB
@Temperature -18.0 °C
NB
@Temperature -0.400 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Melting Point 124.0 °C255.2 °FASTM D3418
Crystallization Temperature 112.5 °C234.5 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 59.5 °C139 °FASTM D648
Vicat Softening Point 116 °C241 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 °C450 °F
Middle Barrel Temperature 243 °C470 °F
Front Barrel Temperature 246 °C475 °F
Nozzle Temperature 246 °C475 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) EX7C HF4750K High Density Polyethylene
Aaron Industries AAROLENE® ARPE HD 300-2 High Density Polyethylene Compounded Resin
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite
LyondellBasell Alathon® ETP H5057 High Density Polyethylene
NIZHNEKAMSKNEFTEKHIM PE 4550N (50401M) High Density Polyethylene

PEQU0786 / 104142

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.