Product Description: DEVELOPMENTAL 15% glass filled, hydrolysis resistant, flame retardant and laser markable black Celanex PBT. Celanex 3216HR ED4222 (LM black) is a flame retarded, hydrolysis resistant, 15% fiberglass reinforced PBT that is enhanced for improved laser marking graphics. It is lasermarkable grade available in an anthrazite color to mark light-color/white. The grade is specially formulated to yield crisp marks when subjected to Nd:YAG laser or equivalent lasers operated at 1064nm or 532nm. Lasers operating in the UV region (355nm) may yield different results. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Filler/Reinforcement: Glass Fiber Additive: Flame Retardant; Hydrolysis Resistant; Lubricant Features: Flame Retardant; Hydrolysis Resistant; Lubricated; Laser Markable Forms: Pellets Processing Method: Injection Molding Information provided by Celanese |