Teflon® PTFE white granular molding powders are ideal for molding many different end products and stock shapes. Excellent chemical resistance, electrical properties, high temperature performance, low temperature toughness, plus unique adhesion and flame resistance. Teflon® PTFE granular molding powders are processed by compressing them into a desired shape and heating them at temperatures above their melting point to consolidate the powder. Resin Characteristics: Presintered resin. These hard, free-flowing particles are useful for ram extrusion processes. Uses: Small diameter rods, tubing, or other profiles for matching or direct use; small parts, such as electrical stand-off or feed-through insulators, lab fittings, or valves. Typical properties for Teflon® PTFE Granular Resin: Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015. |