MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Corning ULE® 7972 Ultra Low Expansion Glass
Categories: Ceramic; Glass; Optical

Material Notes: ULE® Corning Code 7972 Ultra Low Expansion Glass is a titania silicate glass. It is used in applications ranging from machine tool reference blocks to solid and lightweight mirror blanks for large astronomical telescopes and space satellite applications. The mean linear CTE is 0 ± 30 ppb/°C from 5°C to 35°C with a 95% confidence level, and is tested on each boule.

Excellent resistance to weathering. Exhibits virtually no surface clouding or electrical surface leakage when subjected to attack by water, sulfur dioxide, and other atmospheric gases. High resistance to attack by nearly all chemical agents.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.21 g/cc0.0798 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 460460kg/mm² at 200g load
Tensile Strength, Ultimate 49.8 MPa7220 psi
Modulus of Elasticity 67.6 GPa9800 ksi
Bulk Modulus 34.1 GPa4950 ksi
Poissons Ratio 0.170.17
Shear Modulus 29.0 GPa4210 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+11 ohm-cm
@Temperature 200 °C
4.00e+11 ohm-cm
@Temperature 392 °F
100Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  -0.390 µm/m-°C
@Temperature -100 °C
-0.217 µin/in-°F
@Temperature -148 °F
Approximate Instantaneous Value
 -0.180 µm/m-°C
@Temperature -50.0 °C
-0.100 µin/in-°F
@Temperature -58.0 °F
Approximate Instantaneous Value
 -0.0500 µm/m-°C
@Temperature 0.000 °C
-0.0278 µin/in-°F
@Temperature 32.0 °F
Approximate Instantaneous Value
 -0.0300 - 0.0300 µm/m-°C
@Temperature 5.00 - 35.0 °C
-0.0167 - 0.0167 µin/in-°F
@Temperature 41.0 - 95.0 °F
Specified mean from 5 to 35°C
 0.0400 µm/m-°C
@Temperature 150 °C
0.0222 µin/in-°F
@Temperature 302 °F
Approximate Instantaneous Value
 0.0500 µm/m-°C
@Temperature 50.0 °C
0.0278 µin/in-°F
@Temperature 122 °F
Approximate Instantaneous Value
 0.0700 µm/m-°C
@Temperature 100 °C
0.0389 µin/in-°F
@Temperature 212 °F
Approximate Instantaneous Value
Specific Heat Capacity 0.767 J/g-°C
@Temperature 25.0 °C
0.183 BTU/lb-°F
@Temperature 77.0 °F
Thermal Conductivity 1.31 W/m-K
@Temperature 25.0 °C
9.09 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Softening Point 1490 °C2710 °F
Annealing Point 1000 °C1830 °F
Strain Point 890 °C1630 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.4801
@Wavelength 656 nm
1.4801
@Wavelength 656 nm
nC
 1.4828
@Wavelength 589 nm
1.4828
@Wavelength 589 nm
nD
 1.4892
@Wavelength 486 nm
1.4892
@Wavelength 486 nm
nF
Abbe Number 53.153.1vd
 
Descriptive Properties
Stress Optical Coefficient4.15 (nm/cm)/(kg/cm²)
Thermal Diffusivity.0079 cm²/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec Sikor® S Cordierite
CeramTec Sikor® E Cordierite
Aluminum 6082-T6
Aluminum 6063-T5
Schott ZERODUR® Glass Ceramic

CCORNG970 / 233285

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.