MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay BR® 127 Primer with FM 87-1 K Adhesive
Categories: Polymer; Thermoset; Epoxy

Material Notes: BR® 127 corrosion inhibiting primer is a modified epoxy primer. It is a high-performance corrosion inhibiting primer and has been used in many commercial aircraft. BR 127 primer can be used with essentially all 250°F (121°C) film adhesives and has been designed to provide optimal structural performance at temperatures ranging from -67°F to 300°F (-55°C to 149°C). BR 127 primer is formulated to provide maximum environmental resistance and durability within the bond line, as well as prevent corrosive undercutting. It can also be used effectively as a protective coating outside bonded areas. BR 127 corrosion inhibiting primer can be cured prior to bonding. Recommended cure cycles range from 4 hours at 180°F (82°C) to 30 minutes at 250°F (121°C). Articles primed with BR 127 primer and then cured have an indefinite shelf life. Primed details should be wrapped in Kraft paper (as protection from dust and dirt) and stored prior to adhesive bonding. Maintaining controlled conditions of 85°F (29°C) maximum temperature and 65% maximum humidity is recommended for extended storage life. Cure cycles for adhesive films primed with BR 127 primer may vary from 200°F to 350°F (93°C to 177°C) with minimum pressures to assure proper mating of bonded details.

Features & Benefits:

  • Industry-wide standard for corrosion resistant primers
  • Prevents hydrolysis of oxide layers
  • Structural performance from -67°F to 300°F (-55°C to 149°C)
  • Compatible with a wide variety of adhesive systems
  • Improves hydrolytic stability at the adhesive-to-metal interface
  • Protects prepared surfaces from further oxidation
Test Condition: 0.06 psf (300 gsm); Cure Temperature: 1 hour at 250°F (120°C); Service Temperature: 250°F (120°C)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.875 g/cc0.0316 lb/in³BR® 127 Primer
Solids Content 9.0 - 11 %9.0 - 11 %sprayable, BR® 127 Primer
Volatile Organic Compounds (VOC) Content 792 g/l792 g/lBR® 127 Primer
Outgassing - Total Mass Loss 0.48 %0.48 %BR® 127 Primer
Collected Volatile Condensable Material 0.030 %0.030 %BR® 127 Primer
Storage Temperature -18.0 °C-0.400 °FBR® 127 Primer
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  2.62 MPa
@Temperature 120 °C
380 psi
@Temperature 248 °F
Flat-wise; MIL-A-25463B
 4.41 MPa
@Temperature 82.0 °C
640 psi
@Temperature 180 °F
Flat-wise; MIL-A-25463B
 7.24 MPa
@Temperature 24.0 °C
1050 psi
@Temperature 75.2 °F
Flat-wise; MIL-A-25463B
 9.38 MPa
@Temperature -55.0 °C
1360 psi
@Temperature -67.0 °F
Flat-wise; MIL-A-25463B
Shear Strength  18.7 MPa
@Temperature 120 °C
2710 psi
@Temperature 248 °F
Wide area lap; MMM-A-132A
 22.4 MPa
@Temperature 120 °C
3250 psi
@Temperature 248 °F
MMM-A-132A
 28.4 MPa
@Temperature 82.0 °C
4120 psi
@Temperature 180 °F
MMM-A-132A
 29.0 MPa
@Temperature 82.0 °C
4200 psi
@Temperature 180 °F
Wide area lap; MMM-A-132A
 35.9 MPa
@Temperature 24.0 °C
5200 psi
@Temperature 75.2 °F
Wide area lap; MMM-A-132A
 37.9 MPa
@Temperature -55.0 °C
5490 psi
@Temperature -67.0 °F
Wide area lap; MMM-A-132A
 37.9 MPa
@Temperature -55.0 °C
5500 psi
@Temperature -67.0 °F
MMM-A-132A
 46.2 MPa
@Temperature 24.0 °C
6700 psi
@Temperature 75.2 °F
MMM-A-132A
Peel Strength  9.64 kN/m
@Temperature 120 °C
55.0 pli
@Temperature 248 °F
Floating roller; ASTM D3167-76
 10.5 kN/m
@Temperature -55.0 °C
60.0 pli
@Temperature -67.0 °F
Floating roller; ASTM D3167-76
 11.6 kN/m
@Temperature 82.0 °C
66.0 pli
@Temperature 180 °F
Floating roller; ASTM D3167-76
 12.3 kN/m
@Temperature 24.0 °C
70.0 pli
@Temperature 75.2 °F
Floating roller; ASTM D3167-76
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °FStructural performance, as tested
Minimum Service Temperature, Air -55.0 °C-67.0 °FStructural performance, BR® 127 Primer
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthBR® 127 Primer
 
Descriptive Properties
ColorYellow
Honeycomb Sandwich Peel74.1 Nm/mMIL-A-25463B, 120°C
 78.6 Nm/mMIL-A-25463B, -55°C
 87.5 Nm/mMIL-A-25463B, 82°C
 93.4 Nm/mMIL-A-25463B, 24°C
Metal-to-Metal Climbing Drum Peel254 Nm/mASTM D1781-76, 120°C
 280 Nm/mASTM D1781-76, -55°C
 325 Nm/mASTM D1781-76, 24°C
 334 Nm/mASTM D1781-76, 82°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Northern White Pine Wood
Overview of materials for Thermoset Polyurethane Foam, Glass Filled
European Black Pine (Austrian Pine) Wood
Dow 722 Low Density Polyethylene (LDPE)

PCYTED002b / 240079

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.