MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Anderman Ceramics EM60 Mullite
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Synthetic mullite available in rod, tube, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 19".

Information provided by Anderman Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.70 g/cc
Open Porosity 0.00 %Gas Tight
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 8.0
Flexural Strength 23000 psi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+13 ohm-cm
 1.00e+6 ohm-cm
@Temperature 600 °C
Dielectric Constant 6.0
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.50 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 5.00 W/m-K
@Temperature 20.0 - 100 °C
Maximum Service Temperature, Air 1600 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 62 %
CaO 0.18 %
Fe2O3 0.82 %
SiO2 36 %
TiO2 0.39 %
 
Descriptive Properties
Thermal Shock ResistanceExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mullite, 3Al2O3-2SiO2
Anderman Ceramics EA998 Sintered Alumina, 99.8%
CeramTec 701 Cordierite
McDanel Advanced Ceramics MV-30 Mullite
Unifrax Fiberfrax® Fibermax Bulk Mullite High-Temperature Fiber

CANDER00 / 473

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.